The CALCE battery team is open to collaborate with research groups and companies around the world. We provide open access to our experimental test data on lithium-ion batteries, which includes continuous full and partial cycling, storage, dynamic driving profiles, open circuit voltage measurements, and impedance measurements. Battery form factors include cylindrical, pouch, and prismatic, and the chemistries include LCO, LFP, and NMC. The data from these tests can be used for battery state estimation, remaining useful life prediction, accelerated battery degradation modeling, and reliability analysis. A description of each battery and each test is presented below. Use of this data for publication purposes should include references to the CALCE article(s) that describe the experiments conducted to generating the data. If you have questions or are interested to contribute your data to the battery data collective, please contact Prof. Michael Pecht.
| INR 18650-20R Battery | A123 Battery | CS2 Battery | CX2 Battery | PL Sample | Storage Data & Test Description | Accelerated Testing Data | Anomaly Detection Data |
|---|
| Specification | NMC Cell | LFP Cell |
| Capacity | 3500 mAh | 1100 mAh |
| Nominal Voltage | 3.6Vh | 3.2V |
| Cell chemistry | NMC (LiNiMnCoO₂) | LFP (LiFePO₄) |
| Diameter | 18mm | 18mm |
| Length | 65mm | 65mm |
Data and Test Description
This dataset contains experimental measurements of casing strain in commercial 18650 cylindrical lithium-ion cells with nickel manganese cobalt oxide (NMC) and lithium iron phosphate (LFP) chemistries. The experiments investigated how strain-gauge location and orientation affect the measured mechanical response during normal charge–discharge cycling and overcharge.
The measurements include strain, cell voltage, and surface temperature recorded during the experiments. Multiple strain gauges were positioned at different circumferential locations around the cell casing to characterize the spatial distribution of strain. X-ray computed tomography (CT) was also performed to examine the internal jelly-roll configuration, including current-collector tab locations, electrode terminations, and gaps between the jelly roll and the steel casing.
The NMC cell used in this study was an LG INR18650 MJ1 with a nominal capacity of 3500 mAh. Strain measurements were obtained in both hoop and axial orientations. For circumferential characterization, five strain gauges were positioned near the middle of the cell: SG1 directly above the anode tab, SG2 at 90°, SG3 at 180°, SG4 at 270°, and SG5 at 200° clockwise from SG1. Standard charging procedure consisted of constant-current (CC) charging at 1.7 A (approximately 0.5C) to 4.2 V, followed by constant-voltage (CV) charging until the current decreased to 50 mA. Discharging was performed at approximately 0.2C (0.68 A) until the cell voltage reached 2.5 V. Overcharging was conducted at 0.5C.
The LFP cell used in this study was a Golden Cell Power JGPFR18650 with a nominal capacity of 1100 mAh. The LFP cell used in this study was a Golden Cell Power JGPFR18650 with a nominal capacity of 1100 mAh. Standard charge–discharge experiments were conducted at 0.5C. Charging was performed using a constant-current/constant-voltage (CC-CV) protocol with an upper voltage limit of 3.65 V and a charge cut-off current of 11 mA. Discharging was performed at 0.5C until the cell voltage reached 2.5 V. Overcharge was performed at 1C and 1.5C.
The data files contain the recorded measurements corresponding to the respective experiments. Each file includes a README sheet describing the dataset, its measurement channels, and the corresponding figure(s) in the associated research paper.
Top